1,Description of Castable for Cooling Zone:
With high-quality bauxite and corundum fine powder as the main raw materials and alkali-resistant raw materials, the product has good wear resistance, anti-spalling performance, alkali corrosion resistance, non-sticking aluminium products, preventing corundum nodulation, and good use effect.the product forms a ceramic combination in the process of use, with high degree of densification, high strength and good scouring resistance. Alkaline materials resistant to the corrosion of molten aluminum are added to the ingredients to prevent the formation of corundum nodules. In the process of use, it is found that its anti peeling performance is good and does not produce large cracks, which is highly praised by users
2,Index of Castable for Cooling Zone:
JY-3 | ||
Al2O3 | Greater than or equal to 70 | |
Less than or equal to 2.1 | ||
Bulk density g/cm3 | 2.60 | |
110 degree *16h | 8 | |
1200 degree *3h | 10 | |
1400 degree *3h | 12 | |
110 degree *16h | 40 | |
1200 degree *3h | 70 | |
1400 degree *3h | 80 | |
110 degree *16h | -0.05 | |
1200 degree *3h | ±0.2 | |
1400 degree *3h | ±0.5 | |
Greater than or equal to 1790 | ||
2 | ||
1450 | ||
6-8 | ||
2.8 | ||
High strength, wear-resisting, thermal shock resistance, spall-resistance | ||
3,Characteristics of Castable for Cooling Zone:
1)Construction method: pouring
2)Storage Method: Moisture-proof
3)Packaging: Waterproof plastic woven bags are packed and placed on wooden pallets, then tightened
4.Good feedback of product use effect,the products have been exported to Oman,Morocco and India.
5.We are a professional supplier, who can provide customers with free product technology, use and other issues.
Email:wp@cnjingganrefractory.com/sdwenping@163.com
TEL: 86-0533-4188518 / FAX: 86-0533-4188518
Rose:+86-13275332819(wechat/whatsapp number)
الوسم :